NOTE: These values are representative values and do not relate to a specific grade of material
EPDM - Ethylene Propylene Diene Terpolymer
Glass Transition Temperature (°C) -55
Room Temperature Density (°C) 862 <> 892
Maximum Working Temperature (°C) 140
Tensile Strength (MPa) M
Resistance To Tear M
Resistance To Abrasion M
Compression set @ -20°C (%) 20
Compression set @ +23°C (%) 8
Compression set @ +120°C (%) 50
Swelling / 70Hr / ASTM Oil No.3 @ 70°C (%) >140
Swelling / 70Hr / Fuel C @ Room Temperature (%) ---
Gas Permeability M
Ozone Resistance H
Oxidation Resistance VH
Rebound (Hot) VH
Rebound (Cold) VH
Heat Resistance 5 Hours (°C) 200
Heat Resistance 70 Hours (°C) 170
Heat Resistance 1000 Hours (°C) 130
This information reproduced by kind permission of SkidMark Multimedia Productions. E-REF2 is a product of SkidMark Multimedia Productions. © 1994 - 2004