NOTE: These values are representative values and do not relate to a specific grade of material
NR - Natural Rubber
Glass Transition Temperature (°C) -72
Room Temperature Density (°C) 922
Maximum Working Temperature (°C) 100
Tensile Strength (MPa) VH
Resistance To Tear VH
Resistance To Abrasion M/H
Compression set @ -20°C (%) 15
Compression set @ +23°C (%) 8
Compression set @ +120°C (%) 70
Swelling / 70Hr / ASTM Oil No.3 @ 70°C (%) >140
Swelling / 70Hr / Fuel C @ Room Temperature (%) ---
Gas Permeability M
Ozone Resistance L
Oxidation Resistance H
Rebound (Hot) VH
Rebound (Cold) VH
Heat Resistance 5 Hours (°C) 150
Heat Resistance 70 Hours (°C) 120
Heat Resistance 1000 Hours (°C) 90
This information reproduced by kind permission of SkidMark Multimedia Productions. E-REF2 is a product of SkidMark Multimedia Productions. © 1994 - 2004